Compact AlN/Y2O3ceramics were fabricated by combustion synthesis of Al particles in the super high pressure nitrogen(1000atm).In the SHS process of AlN2 Y2O3 system,when the temperature was up to 1760℃,eutectic melt Y3Al5O12was formed from Y2O3and Al2O3,then liquid sinter occurred With increasing of Y2O3content in the original powder system, porosity of the products decreased,content of the plastic Al in the products increased, then bending strength and fracture toughness increased In AlN2Y2O3>system, SHS densification have apparent tropism, mainly occurred along the combustion front.
Key words
AlN ceramic /
combustion synthesis /
Y2O33 /
densification /
SHS HIP
{{custom_keyword}} /
{{custom_sec.title}}
{{custom_sec.title}}
{{custom_sec.content}}
References
[1] Laurel M.Sheppard.Am.Cera.Bull,1990,69(11):1801~1812
[2] Y.Baik et al.Key Engineering,1996,122~124:553~570
[3] A.G.Merzhanov.Particulate Materials and Processes:Advances in Powder Metallurgy & Particalate Materials,Princeton,NJ.1992(6),341~367
[4] 李凝芳,周毅.材料导报,1994,2:38~43
[5] 江国健等.无机材料学报,1998,13(1):105~108
[6] 陈克新.博士论文,北京科技大学,1997:30~68
{{custom_fnGroup.title_en}}
Footnotes
{{custom_fn.content}}