Please wait a minute...
 
材料工程  2005, Vol. 0 Issue (4): 60-63    
  综述 本期目录 | 过刊浏览 | 高级检索 |
Cf/SiC陶瓷基复合材料的发展与应用现状
张玉娣, 周新贵, 张长瑞
国防科技大学航天与材料工程学院先进陶瓷纤维及其复合材料重点实验室, 长沙, 410073
Development and Application of Cf/SiC Ceramic Matrix Composites
ZHANG Yu-di, ZHOU Xin-gui, ZHANG Chang-rui
Key Laboratory of Advanced Ceramic Fibers and Composites, College of Aerospace and Materials Engineering, National University of Defense Technology, Changsha 410073, China
全文: PDF(179 KB)   HTML()
输出: BibTeX | EndNote (RIS)      
摘要 介绍了Cf/SiC复合材料的制备工艺,分析了各种制备工艺的优、缺点。描述了Cf/SiC复合材料近年来在航空涡轮发动机、热保护系统、光学结构及光学反射镜以及刹车片系统等领域的应用发展状况。对当前Cf/SiC复合材料研究存在的问题进行了分析,指出提高Cf/SiC陶瓷基复合材料抗氧化性仍是未来发展的一个重要研究方向。
服务
把本文推荐给朋友
加入引用管理器
E-mail Alert
RSS
作者相关文章
张玉娣
周新贵
张长瑞
关键词 陶瓷基复合材料Cf/SiC工艺应用    
Abstract:The several fabrication processes of Cf/SiC ceramic matrix composite(CMC) were introduced.The advantage and disadvantage of every process was analyzed.The discussion was put emphasis on development and application of Cf/SiC composite,such as aeronautic turbine engine,thermal protective system,optical structure and mirror,brake system and so on.Some current problems that lie in study of Cf/SiC composites were analyzed,it was put forward that how to improve the oxygenation resistance of Cf/SiC composites is still an important research and development direction in the future.
Key wordsCMC    Cf/SiC    process    application
收稿日期: 2003-08-25      出版日期: 2005-04-20
中图分类号:  TQ34.74  
作者简介: 张玉娣(1976- ),女,博士研究生,主要研究方向为陶瓷基复合材料,联系地址:湖南长沙国防科技大学航材院重点实验室(410073).
引用本文:   
张玉娣, 周新贵, 张长瑞. Cf/SiC陶瓷基复合材料的发展与应用现状[J]. 材料工程, 2005, 0(4): 60-63.
ZHANG Yu-di, ZHOU Xin-gui, ZHANG Chang-rui. Development and Application of Cf/SiC Ceramic Matrix Composites. Journal of Materials Engineering, 2005, 0(4): 60-63.
链接本文:  
http://jme.biam.ac.cn/new/CN/      或      http://jme.biam.ac.cn/new/CN/Y2005/V0/I4/60
[1] [日] 宗保重行.近代陶瓷[M]. 上海:同济大学出版社,1988.
[2] 何新波,杨辉,张长瑞,等.先驱体转化-热压烧结Cf/SiC 复合材料的致密化机理[J].材料科学与工程,2002,20(3):358-360,370.
[3] 何新波,杨辉,张长瑞,等.连续纤维增强陶瓷基复合材料概述[J].材料科学与工程,2002,20(2):273-278,262.
[4] NAKANO,KIKUO.Fabrication and mechanical properties of carbon fiber-reinforced silicon carbide composites[J]. Journal of the Ceramic Society of Japan,1992,100(4):472-475.
[5] 王零森,黄培云.特种陶瓷[M].长沙:中南工业大学出版社,1994.
[6] 梁波.反应合成法制备先进陶瓷[J].材料科学与工艺,2000,8(3):84-87.
[7] 朱时珍,李俊红,于晓东.连续碳纤维增强碳化硅复合材料的制备与性能研究[J].北京理工大学学报,2002,22(4):422-425.
[8] SANOKAWA YUTAKA.Application of continuous fiber reinforced silicon carbide matrix composites to a ceramic gas turbine model for automobiles[J].Ceram Eng Sci Proc,1997,(4):221-228.
[9] 徐立同.CVI法制备三维碳纤维增强碳化硅陶瓷基复合材料[J].硅酸盐学报,1996,24(10):485-489.
[10] HARNISCH B.Ultralight weight C/SiC mirrors and structures[J]. ESA Bulletin 95,1998,(8):148-152.
[11] DURAN A, APARICIO M.Reinfiltration processes for polymer derived fiber reinforced ceramics[J].Key Engineering Materials,1997, 127-131(1):287-294.
[12] 马青松,陈朝辉,郑文伟, 等.先驱体转化法制备连续纤维增强陶瓷基复合材料的研究[J]. 材料科学与工程, 2001,19(4):110-115,121.
[13] 马江.先驱体液相浸渍工艺制备纤维增强碳化硅基复合材料[D].长沙:国防科技大学,2000.
[14] ORTONA A.SiC-SiCf CMC manufacturing by hybrid CVI-PIP techniques:process optimization[J].Fusion Engineering and Design, 2000, 51-52:159-163.
[15] 宋麦丽,王涛.高性能C/SiC复合材料的快速制备[J].新型碳材料,2001,16(2):57-60.
[16] 葛明龙,田昌义,孙纪国.碳纤维增强复合材料在国外液体火箭发动机上的应用[J].导弹与航天运载技术,2003,264(4):22-26.
[17] ECKEL A J.Thermal shock fiber reinforced ceramic matrix composites[J]. Ceram Eng Sci Proc, 1991,73(7-8):1500-1508.
[18] TRABANDT U, WULZ H G, SCHMID T. CMC for hot structures and control surfaces of future launchers[J]. Key Engineering Mater, 1999, 164-165:445-450.
[19] IMUTA M, GOTOH J. Development of high temperature materials including CMCs for space application[J]. Key Engineering Mater, 1999, 164-165:439-444.
[20] HERBELL, THOMAS P.Composites in high speed turbines for rocket engines[A].High temperature high performance materials for rocket engines and space application proceeding[M].Warredale:Minerals,Metals and Materials Soc(TMS),1995.13-20.
[21] 戴钺.C/SiC 复合材料连接到金属上[J].现代材料动态,2000,(7):14.
[22] CLAUS MULLER,ULRICH PAPENBURG.C/SiC high precision lightweight components for optomechanical applications[M]. Bellingham:The International Society for Optical Engineering(SPIE), 2001.
[23] PAPENBURG U.Optical and optomechanical ultra-light wei-ght C/SiC components[A].SPIE International Symposium on Optical Science, Engineering,and Instruments[C].Denver:The International Society for Optical Engineering(SPIE), 1999.126-131.
[1] 徐晨曦, 胡安俊, 舒朝著, 龙剑平. 金属相二硫化钼在能量储存与转化中的应用进展[J]. 材料工程, 2020, 48(9): 34-46.
[2] 叶锦宗, 李锦棒, 周宁宁, 曹均, 卿涛, 蒋世宇, 于爱兵. 成型工艺对多孔PI材料摩擦学及力学性能的影响[J]. 材料工程, 2020, 48(9): 144-151.
[3] 包建文, 钟翔屿, 张代军, 彭公秋, 李伟东, 石峰晖, 李晔, 姚锋, 常海峰. 国产高强中模碳纤维及其增强高韧性树脂基复合材料研究进展[J]. 材料工程, 2020, 48(8): 33-48.
[4] 肇研, 刘寒松. 连续纤维增强高性能热塑性树脂基复合材料的制备与应用[J]. 材料工程, 2020, 48(8): 49-61.
[5] 刘雪峰, 白于良, 李晶琨, 秦回一, 陈鑫. 冷轧成形钛/钢层状复合板界面结合强度的影响因素[J]. 材料工程, 2020, 48(7): 119-126.
[6] 刘兴华, 王军丽, 王亚玲, 张利, 杨永珍, 刘旭光. 多色荧光碳点调控及其应用[J]. 材料工程, 2020, 48(4): 36-45.
[7] 戚云超, 方国东, 梁军, 谢军波. 三维针刺C/C-SiC复合材料预制体工艺参数优化[J]. 材料工程, 2020, 48(1): 27-33.
[8] 王晓辉, 罗海文. 飞机起落架用超高强度不锈钢的研究及应用进展[J]. 材料工程, 2019, 47(9): 1-12.
[9] 周莉, 柳汀, 郑典亮, 许勇刚. 选择表面工艺改性的CIPs涂层及其氧化物的吸波性能[J]. 材料工程, 2019, 47(9): 132-138.
[10] 高晔, 焦健. NITE工艺制备SiCf/SiC复合材料的研究进展[J]. 材料工程, 2019, 47(8): 33-39.
[11] 张世杰, 王汝敏, 刘宁, 廖英强, 程勇. 纺丝工艺对T800碳纤维及其复合材料性能的影响[J]. 材料工程, 2019, 47(8): 118-124.
[12] 周怡然, 刘虎, 杨金华, 姜卓钰, 吕晓旭, 焦健. 熔融渗透工艺制备SiC-TiSi2复相陶瓷的反应机理[J]. 材料工程, 2019, 47(6): 88-93.
[13] 李雅莉, 雷力明, 侯慧鹏, 何艳丽. 热工艺对激光选区熔化Hastelloy X合金组织及拉伸性能的影响[J]. 材料工程, 2019, 47(5): 100-106.
[14] 宋仁国. 微弧氧化技术的发展及其应用[J]. 材料工程, 2019, 47(3): 50-62.
[15] 刘巧沐, 黄顺洲, 何爱杰. 碳化硅陶瓷基复合材料在航空发动机上的应用需求及挑战[J]. 材料工程, 2019, 47(2): 1-10.
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
版权所有 © 2015《材料工程》编辑部
地址:北京81信箱44分箱 邮政编码: 100095
电话:010-62496276 E-mail:matereng@biam.ac.cn
本系统由北京玛格泰克科技发展有限公司设计开发 技术支持:support@magtech.com.cn