稀土Y,Ce对K418镍基高温合金微观组织的影响
金玉花, 韩萍花, 李常锋, 寇生中
兰州理工大学甘肃省有色金属新材料省部共建国家重点实验室, 兰州 730050
Effect of Rare Earth Elements (Y,Ce) on Microstructure of K418 Ni-base Superalloy
JIN Yu-hua, HAN Ping-hua, LI Chang-feng, KOU Sheng-zhong
State Key Laboratory of Advanced Processing and Recycling of Nonferrous Metals, Lanzhou University of Technology, Lanzhou 730050, China
全文: PDF(11154 KB)   HTML()
输出: BibTeX | EndNote (RIS)      
摘要 采用高真空电弧熔炼炉熔炼,制备了K418镍基高温合金。借助SEM对合金的组织进行观察,用EDS对合金中的相成分进行分析,研究了稀土元素Y,Ce对合金中气孔缺陷、γ'相以及(γ+γ')共晶相等的影响。结果表明:添加稀土元素明显减少了合金中的气孔缺陷,提高了合金的致密度,细化了合金枝晶组织。组织中碳化物的形态由大块状变为链状和小块状,γ'相尺寸变小且颗粒数目增多。 Y元素的加入能使合金中的(γ+γ')共晶相数目增加。但同时加入Y,Ce两种稀土元素后共晶相数目的增加更为显著。
服务
把本文推荐给朋友
加入引用管理器
E-mail Alert
RSS
作者相关文章
金玉花
韩萍花
李常锋
寇生中
关键词 K418合金稀土元素&gamma'相共晶相    
Abstract:K418 Ni-base superalloy was melted in high vacuum arc-melting furnace. The microstructure was observed by using SEM, the phase composition was detected by EDS. The effect of with rare earth elements on pore defects, γ' phase and eutectic phase of the alloy was studied and the effect mechanism was analyzed. The results show that the pore defects of the alloy decrease with the addition of rare earth elements, the density increases, the dendritic structure is refined. The morphology of carbides in alloy turns from bulk into chain and small pieces, the γ' phase in alloy with the addition of rare earth elements becomes smaller in size and much more in numbers. The eutectic phase(γ+γ') volume remarkably increases with the addition of Y, however the eutectic phase volume increases more obviously if two rare earth elements Y, Ce are added simultaneously.
Key wordsK418 superalloy    rare earth element    &gamma    ' phase    eutectic phase
收稿日期: 2014-07-31      出版日期: 2016-03-22
中图分类号:  TG146.1+5  
通讯作者: 金玉花(1978-),女,博士,副教授,硕士研究生导师,主要从事有色金属连接技术的科研与教学工作,联系地址:甘肃省兰州市兰州理工大学材料学院(730050),E-mail:yhjin8686@163.com     E-mail: yhjin8686@163.com
引用本文:   
金玉花, 韩萍花, 李常锋, 寇生中. 稀土Y,Ce对K418镍基高温合金微观组织的影响[J]. 材料工程, 2016, 44(3): 46-51.
JIN Yu-hua, HAN Ping-hua, LI Chang-feng, KOU Sheng-zhong. Effect of Rare Earth Elements (Y,Ce) on Microstructure of K418 Ni-base Superalloy. Journal of Materials Engineering, 2016, 44(3): 46-51.
链接本文:  
http://jme.biam.ac.cn/CN/10.11868/j.issn.1001-4381.2016.03.008      或      http://jme.biam.ac.cn/CN/Y2016/V44/I3/46
[1] MAHOBIA G S, PAULOSE N, MANNAN S L, et al. Tensile behavior of alloy 718 in hot corrosive environment[J]. Journal of Materials Engineering and Performance, 2013, 22(12):3810-3817.
[2] 石照夏,董建新,张麦仓. K418合金显微组织及其增压器涡轮叶片热裂的研究[J]. 稀有金属材料与工程, 2012, 41(11):1935-1939. SHI Zhao-xia, DONG Jian-xin, ZHANG Mai-cang.Research on microstructure of K418 alloy and hot tearing of its turbocharger turbine blades[J]. Rare Metal Materials and Engineering, 2012, 41(11):1935-1939.
[3] LONG F L, YA L D. A new current hybrid inertia friction welding for nickel-based superalloy K418-alloy steel 42CrMo dissimilar metals[J]. Int J Adv Manuf Technol, 2014, 70:1673-1681.
[4] 王伟, 李强, 杨维才, 等. 镍基铸造高温合金的热等静压改性研究[J]. 金属热处理, 2014, 39(1):85-88. WANG Wei, LI Qiang, YANG Wei-cai, et al. Modification of cast nickel-base superalloy by hot isostatic pressing[J]. Heat Treatment of Metals, 2014, 39(1):85-88.
[5] KO D H, KANG B H, KO D C, et al. Improvement of mechanical properties of Al6061 extrudate by die cooling with N2 gas during hot extrusion[J]. Journal of Mechanical Science and Technology, 2013, 27(1):153-161.
[6] 牛建平, 杨克怒. 采用CaO坩埚超纯净熔炼Ni基高温合金[J]. 机械工程材料, 2001, 25(5):19-20. NIU Jian-ping, YANG Ke-nu. The super refining of Ni-base superalloy using CaO crucible[J]. Materials for Mechanical Engineering, 2009, 27(6):822-828.
[7] 谷怀鹏, 刘丽君, 曹腊梅, 等. 含Ru镍基单晶高温合金的显微组织和拉伸性能研究[J]. 航空材料学报, 2013, 33(6):20-26. GU Huai-peng, LIU Li-jun, CAO La-mei, et al. Microstructure and tensile property of Ru-containing Ni base single crystal superalloy[J]. Journal of Aeronautical Materials, 2013, 33(6):20-26.
[8] 杨海青, 李青, 肖程波, 等. Re及时效时间对耐腐蚀镍基定向合金组织和持久寿命的影响[J]. 材料工程, 2015, 43(6):31-37. YANG Hai-qing, LI Qing, XIAO Cheng-bo, et al. Effect of Re and aging time on microstructure and stress rupture life of corrosion resistance directionally solidified Ni-base superalloy[J]. Journal of Materials Engineering, 2015, 43(6):31-37.
[9] 郭建亭. 几种微量元素在高温合金中的作用与机理[J]. 中国有色金属学报, 2011, 21(3):465-475. GUO Jian-ting. Effects of several minor elements on superalloys and their mechanism[J]. The Chinese Journal of Nonferrous Metals, 2011, 21(3):465-475.
[10] 肖旋, 赵海强, 郭建亭, 等. B和P对GH 984合金组织和力学性能的影响[J]. 金属学报, 2013, 49(4):421-427. XIAO Xuan, ZHAO Hai-qiang, GUO Jian-ting. et al. Effect of B and P on microstructure and mechanical properties of GH984 alloy[J]. Acta Metallurgica Sinica, 2013, 49(4):421-427.
[11] SHENG L Y, GUO J T, YUAN C, et al. Investigation on B, Cr doped Ni3Al alloy prepared by self-propagation high-temperature synthesis and hot extrusion[J]. Materials Science Forum, 2013, 747:124-131.
[12] ZHOU P, YU J, SUN X, et al. Roles of Zr and Y in cast microstructure of M951 nickel-based superalloy[J]. Transactions of Nonferrous Metals Society of China, 2012, 22(7):1594-1598.
[13] 周鹏杰, 何向明. 微量元素对镍基高温合金共晶数量的影响[J]. 铸造, 2012, 61(8):868-872. ZHOU Peng-jie, HE Xiang-ming. Influences of minor alloying elements on the eutectic volume of Ni-base superalloy[J]. Foundry, 2012, 61(8):868-872.
[14] 梁补女,张振宇. 含稀土元素的Fe-Ni-RE粉末冶金材料的研究[J]. 新技术新工艺, 2005,(9):52-54. LIANG Bu-nü, ZHANG Zhen-yu. Development of P/M Fe-Ni-RE material containing rare-earth elements[J]. New Technology and New Process, 2005,(9):52-54.
[15] 彭志江, 李志军, 侯介山, 等. 钇, 铈对低铪镍基K444返回合金组织与力学性能的影响[J]. 中国稀土学报, 2009, 27(6):822-828. PENG Zhi-jiang, LI Zhi-jun, HOU Jie-shan, et al. Effect of yttrium and cerium on microstructures and mechanical properties of revert Ni-base superalloy K444 with low hafnium content[J]. Journal of the Chinese Rare Earth Society, 2009, 27(6):822-828.
[16] 田宁, 田素贵, 于慧臣, 等. DZ125镍基合金蠕变期间的组织演化与元素扩散迁移率[J]. 中国有色金属学报, 2014, 24(2):335-342. TIAN Ning, TIAN Su-gui, YU Hui-chen, et al. Microstructure evolution and element diffusion mobility of DZ125 nickel-based superalloy during creep[J]. The Chinese Journal of Nonferrous Metals, 2014, 24(2):335-342.
[17] 郭建亭. 高温合金材料学(上册)[M]. 北京:科学出版社, 2008. GUO Jian-ting. Materials Science and Engineering for Superalloys (I)[M]. Beijing:Science Press, 2008.
[18] 王明罡, 田素贵, 于兴福, 等. Re及温度对单晶镍基合金晶格常数及错配度的影响[J]. 稀有金属材料与工程, 2010, 39(2):268-272. WANG Ming-gang, TIAN Su-gui, YU Xing-fu, et al. Influences of element Re and temperatures on the lattice parameter and misfit of single-crystal nickle-base superalloys[J]. Rare Metal Materials and Engineering, 2010, 39(2):268-272.
[1] 黄高仁, 孙乙萌, 张利, 刘玉林. 微量Ce对亚快速凝固Al-Zn-Mg-Cu合金组织与性能的影响[J]. 材料工程, 2018, 46(3): 105-111.
[2] 屈敏, 刘鑫, 崔岩, 刘峰斌, 焦志伟, 刘园. 稀土元素对原位合成TiB2/Al复合材料组织和性能的影响[J]. 材料工程, 2018, 46(3): 98-104.
[3] 黄高仁, 孙乙萌, 张利, 刘玉林. Ce对Al-Zn-Mg-Cu合金亚快速凝固铸造组织的影响[J]. 材料工程, 2017, 45(11): 102-107.
[4] 郭丰伟, 康永旺, 肖程波. 稀土元素(La,Sm,Tb)合金化铌硅材料显微组织及室温断裂韧度[J]. 材料工程, 2016, 44(10): 8-16.
[5] 杨万鹏, 胡本芙, 刘国权, 吴凯. 高性能镍基粉末高温合金中γ'相形态致锯齿晶界形成机理研究[J]. 材料工程, 2015, 43(6): 7-13.
[6] 明宪良, 陈静, 谭华, 杨海欧, 林鑫. 激光立体成形GH4169高温合金γ"相的高温粗化行为[J]. 材料工程, 2014, 0(8): 8-14.
[7] 王定刚, 肖程波, 宋尽霞, 李青, 余乾. 不同稀土元素添加量对K465合金微观组织与力学性能的影响[J]. 材料工程, 2014, 0(8): 46-50.
[8] 王新星, 张宝林, 王行展, 冯凌云. 雾化热分解-氧化五羰基铁制备磁性氧化铁纳米粒子[J]. 材料工程, 2014, 0(8): 51-54.
[9] 刘鹏, 江海涛, 段晓鸽, 康强. 稀土元素Y和Ce对热轧Mg-1.5Zn镁合金组织和室温成形性能的影响[J]. 材料工程, 2014, 0(12): 1-10.
[10] 岳丽杰, 王龙妹, 陈蕴博. 稀土对耐候钢耐蚀性能的影响研究[J]. 材料工程, 2009, 0(3): 74-77,81.
[11] 龚晓钟, 汤皎宁, 李均钦, 梁文涛. 非水体系电沉积稀土填充半导体热电材料Bi2Sb3Lax及其电性能研究[J]. 材料工程, 2008, 0(5): 29-33,38.
[12] 龚晓钟, 汤皎宁, 李均钦, 周莉, 张宇, 辛亚飞. 电化学方法制备单一稀土金属钆薄膜[J]. 材料工程, 2007, 0(1): 37-41,46.
[13] 丁胜, 李宁, 胥永刚, 邱绍宇, 邹红, 李聪. 稀土对Fe-17.5Mn合金阻尼性能的影响[J]. 材料工程, 2006, 0(9): 17-19.
[14] 郭建亭, 任维丽, 周继扬. 稀土元素在金属间化合物(铝化物)中的作用[J]. 材料工程, 2002, 0(1): 36-39,43.
[15] 王淑荷, 郭建亭, 赖万慧, 谭明晖, 李辉, 殷为民. 微量Y对铸造Ni50Al20Fe30合金组织与性能的影响[J]. 材料工程, 1999, 0(7): 43-46.
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
版权所有 © 2015《材料工程》编辑部
地址:北京81信箱44分箱 邮政编码: 100095
电话:010-62496276 E-mail:matereng@biam.ac.cn
本系统由北京玛格泰克科技发展有限公司设计开发 技术支持:support@magtech.com.cn