众所周知,各种断口的宏观或微观形貌都是与特定的断裂机理相关的.人们往往通过断口的宏观和微观形貌的观察来推断零件断裂的某些原因,探讨断裂的机理. 合金断口的宏观和微观形貌,除与应力状态、温度和环境有关外,还与合金的析出相密切相关.
{{custom_sec.title}}
{{custom_sec.title}}
{{custom_sec.content}}
参考文献
[1] 镍基高温合金的典型组织,航空材料专集(1),1977.50
[2] 四种高钨类型铸造镍基高温合金的组织和性能,上海钢铁研究所、北京钢铁研究院、三机部六二一所,1977.5.
[3] C.T.Sims,Superaloys,P.259-284.
[4] R.L.Dreshfield and R.L.Ashbrook,Sigma Phase Formation and its Effect on Stress-rupture Properties of IN-100, NASA-TN-D-5185.1969.
[5] R.L.Dreshfield and R.L.Ashbrook,Effects Sigma Phase Formation on Some Mechanical Properties of Wrought Nickel-Base Superalloy(IN-l00),NASA-TN-D-7654,1974.
[6] ASM Transaction Quarterly.1966,Vol.59, No3,P.505-516.
[7] Physica Status Solidi,1969,Vol.35,No 1,P.11.
[8] μ相的形成及其对机械性能的影响,六二一所(待发表).
[9] R.R.Sahm and M.O.Speidal,High-temperature Materials in Gas Turbine.1974.
{{custom_fnGroup.title_cn}}
脚注
{{custom_fn.content}}